Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.65 GPa | 674 ksi | ASTM D790 |
PolyOne Nymax™ GBF 1200 23 HS BLACK 18 Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Flexural Modulus | 4.65 GPa | 674 ksi | ASTM D790 |
Nylene® PA6/6 Glass Filled 5113 HS Nylon 6/6 13% Glass Filler; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Flexural Modulus | 4.65 GPa | 674 ksi | ASTM D790 |
PTS Trimid® N66-G13 13% Glass Fiber Reinforced Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 4.65 GPa | 674 ksi | ASTM D790 |
Penn Fibre Pennite® 4512 Nylon 6, 12% Glass Fiber Reinforced (PA6) PENNITE® 4512 is a 12% glass fiber reinforced, black pigmented, thermally modified, type 6 nylon, available in sheets and rolls for high performance thermoforming and fabrication applications. PENN.. |
|||
Flexural Modulus | 4.65 GPa | 674 ksi | ASTM D790 |
LNP Thermocomp® JF-1004 EM M BK905 Polyethersulfone, Milled Glass Fiber
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Flexural Modulus | 4.65 GPa | 674 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF PX07437 PA 6 Compound based on Nylon 6 resin containing glass fiber and impact modifier. |
|||
Flexural Modulus | 4.65 GPa | 674 ksi | ASTM Test |
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Dry) Ultramid 8272G HS BK-102 is a 12% glass fiber reinforced, black pigmented, thermally modified, nylon 6 blow molding compound offering an excellent balance of engineering properties combined with the.. |