Polymer Property : Flexural Modulus = 7.25 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0500 GPa
7.25 ksi
ISO 178
Huntsman AVALON® 92 AB Thermoplastic Polyurethane
Introduction: AVALON 92 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 92 AB is part of the AVALON Performance Range and offers a premium soling ma..
Flexural Modulus 0.0500 GPa
7.25 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCD771 PPE-TPE (Asia Pacific)
Flexible, high tensile elongation, halogen-free extrusion grade intended for evaluation in applications such as cable jacket. Flame retardant performance capable of meeting UL VW-1 requirement. 80C ..
Flexural Modulus 0.0500 GPa
7.25 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCD883 PPE-TPE
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as jacket of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN 502..
Flexural Modulus 0.0500 GPa
7.25 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCD883 PPE-TPE (Asia Pacific)
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as jacket of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN 502..
Flexural Modulus 0.0500 GPa
7.25 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCP700 PPE-TPE
Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness.
Flexural Modulus 0.0500 GPa
7.25 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCP700 PPE-TPE
Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness.
Flexural Modulus 0.0500 GPa
7.25 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCP700 PPE-TPE (Asia Pacific)
Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness.
Flexural Modulus 0.0500 GPa
7.25 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCP700 PPE-TPE (Asia Pacific)
Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness.
Flexural Modulus 0.0500 GPa
7.25 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCP700 PPE-TPE (Europe-Africa-Middle East)
Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness.
Flexural Modulus 0.0500 GPa
7.25 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCP700 PPE-TPE (Europe-Africa-Middle East)
Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness.
Flexural Modulus 0.0500 GPa
7.25 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCP761 PPE-TPE
Flexible Noryl injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain re..
Flexural Modulus 0.0500 GPa
7.25 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCP761 PPE-TPE (Asia Pacific)
Flexible Noryl injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain re..
Flexural Modulus 0.0500 GPa
7.25 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCD883 PPE-TPE (Europe-Africa-Middle East)
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as jacket of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN 502..
Flexural Modulus 0.0500 GPa
7.25 ksi
ISO 178
DuPont Performance Polymers Hytrel® RS 40F3 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Renewably Sourced High Flow Polyester Elastomer Developed for Injection Molding Hytrel RS 40F3 NC010 is a high flow low modulus grade containing at least 50% renewably sourced ingredients..
Flexural Modulus 0.0500 GPa
7.25 ksi
ISO 178
DuPont Performance Polymers Hytrel® RS 40F5 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Renewably Sourced Medium Viscosity Polyester Elastomer Information provided by DuPont Performance Polymers
Flexural Modulus 0.0500 GPa
7.25 ksi
ASTM D638
Arkema Group LOTRYL® 18 MA 02 Copolymer Ethylene - Methyl Acrylate
LOTRYL® 18 MA 02 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the methyl acrylate content, LOTRYL® 18 MA 02 is a polymer of ..
Flexural Modulus 0.0500 GPa
7.25 ksi
ASTM D638
Arkema Group LOTRYL® 15 MA 03 Copolymer Ethylene - Methyl Acrylate
LOTRYL® 15 MA 03 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the methyl acrylate content, LOTRYL® 15 MA 03 is a polymer of ..
Flexural Modulus 0.0500 GPa

@Thickness 2.00 mm
7.25 ksi

@Thickness 0.0787 in
molded plaque, cured 20 hr at 100°C; ASTM D790
BASF Elastollan® 1190A10 Wire & Cable Grade Polyurethane Elastomer
As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.