Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.20 - 7.72 GPa | 899 - 1120 ksi | Average value: 7.12 GPa Grade Count:7 |
Overview of materials for Phenolic, Novolac, Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o.. |