Mechanical Properties Metric English Comments
Flexural Modulus 4.00 - 5.00 GPa
580 - 725 ksi
Transverse
Quadrant Plastic Composites MultiQ® Concrete Thermoplastic Panel Composite
MultiQ is a product line of thermoplastic composites in panel form whose specific properties make them particularly suitable as an environmental alternative to plywood in outdoor applications. Howev..
Flexural Modulus 3.50 - 5.00 GPa

@Temperature 60.0 - 120 °C
508 - 725 ksi

@Temperature 140 - 248 °F
Average value: 4.03 GPa Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..
Flexural Modulus 4.00 - 5.00 GPa
580 - 725 ksi
ASTM D790
Chang Chun Plastic PBT3015 15% Glass Fiber Enforced PBT
Information provided by Dowell Trading Company Ltd.
Flexural Modulus 2.50 - 5.00 GPa

@Temperature 60.0 - 120 °C
363 - 725 ksi

@Temperature 140 - 248 °F
Average value: 3.67 GPa Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..