Techmer ES HiFill® PA4/6 M/GF 20 HS 20% Glass/Mineral Filled

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Glass Fiber Reinforced
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA4/6 M/GF 20 HS 20% Glass/Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
Water Absorption 2.6 %

@Time 86400 sec
2.6 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 119 MPa
17200 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Strength 172 MPa
25000 psi
ASTM D790
Flexural Modulus 5.03 GPa
730 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 73.8 µm/m-°C
41.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 285 °C
545 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
ASTM D257
Dielectric Strength 27.6 kV/mm
700 kV/in
Method A (Short-Time); ASTM D149