Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.25 GPa | 1340 ksi | ISO 178 |
PTS PBT-6630 30% Glass Filled PBT6630 is an injection molding grade, with 30% glass fiber reinforced, high heat stability, and electrical properties, easy to process. It is widely used in automotive, home appliance, Electrical i.. |
|||
Flexural Modulus | 9.25 GPa | 1340 ksi | ASTM D790 |
SABIC Innovative Plastics LNP KONDUIT ITF2B PA 6/12 (Asia Pacific) LNP* Konduit* ITF2B is a compound based on Nylon 6/12 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Flexural Modulus | 9.25 GPa | 1340 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2310F PEI 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Flexural Modulus | 9.25 GPa | 1340 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU2300 PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Flexural Modulus | 9.25 GPa | 1340 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU2310 PEI 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Flexural Modulus | 9.25 GPa | 1340 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU2310 PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Flexural Modulus | 9.25 GPa | 1340 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU2310 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Flexural Modulus | 9.25 GPa | 1340 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX99873C PC LNP STAT-KON* DX99872C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Flexural Modulus | 9.25 GPa | 1340 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PF008 PA 6 LNP THERMOCOMP* PF008 is a compound based on Nylon 6 resin containing 40% Glass Fiber. |
|||
Flexural Modulus | 9.25 GPa | 1340 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PF008S PA 6 LNP THERMOCOMP* PF008S is a compound based on Nylon 6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 9.25 GPa | 1340 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PF008S PA 6 (Asia Pacific) LNP THERMOCOMP* PF008S is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 9.25 GPa | 1340 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF006SXZ PA 66 LNP* THERMOCOMP* RF006SXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this material is: Heat Stabilized. |
|||
Flexural Modulus | 9.25 GPa | 1340 ksi | Method I (3 point load), Injection Molded; ISO 178; ASTM D790 |
Styron DLGF9411.00 Polypropylene Overview: DLGF 9400.00 is a 40% long glass fiber reinforced grade with good flow properties. The glass fibers (12 mm length) are coupled to the polypropylene matrix resulting in high stiffness and s.. |
|||
Flexural Modulus | 9.25 GPa | 1340 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PF008 PA 6 (Asia Pacific) LNP THERMOCOMP* PF008 is a compound based on Nylon 6 resin containing Glass Fiber. |
|||
Flexural Modulus | 9.25 GPa | 1340 ksi | ASTM-D790 |
Polyram Polytron A30B041 Nylon 66, 30% Long Fiber 30% LONG FIBER GLASS REINFORCED, PTFE LUBRICATED, UV STABILIZED BLACK NYLON 6.6 FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 9.25 GPa | 1340 ksi | ISO 178 |
BLUESTAR PBT 6630 30% Glass Filled PBT6630 is an injection molding grade, with 30% glass fiber reinforced, high heat stability, and electrical properties, easy to process. It is widely used in automotive, home appliance, E/E industry.. |