Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.25 GPa | 906 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp FF008L PE LNP* Thermocomp* FF008L is a compounding based on Polyethylene containing glass fiber. Added characteristics include Low Extractible.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 6.25 GPa | 906 ksi | ASTM D790 |
Zhejiang Double Fish YS-G030 30% Long Fiber Glass Reinforced Polypropylene Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm.. |
|||
Flexural Modulus | 6.25 GPa | 906 ksi | ISO 178 |
Ecomass® 1950ZC84 Stainless Steel Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsStainless Steel Powder Filled Polyamide (PA6/10)Very Good ToughnessInformation provided by Technical Polym.. |
|||
Flexural Modulus | 6.25 GPa | 906 ksi | |
Budd Hi-Flex® SMC
(discontinued **) Parts requiring high strength and dimensional stability, excellent surface smoothness without sink marks; parts to be painted requiring an automotive-type finish.Data provided by the manufacturer. |