Ecomass® 1950ZC84 Stainless Steel Filled Polyamide

Category Polymer , Thermoplastic , Nylon , Nylon 610
Manufacturer Ecomass Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ecomass® 1950ZC84 Stainless Steel Filled Polyamide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsStainless Steel Powder Filled Polyamide (PA6/10)Very Good ToughnessInformation provided by Technical Polymers
Physical Properties Metric English Comments
Specific Gravity 3.80 g/cc
3.80 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
Internal
Mechanical Properties Metric English Comments
Tensile Strength at Break 27.0 MPa
3920 psi
ISO 527
Elongation at Break 0.50 %
0.50 %
ISO 527
Tensile Modulus 7.583 GPa
1100 ksi
ISO 527
Flexural Modulus 6.25 GPa
906 ksi
ISO 178
Izod Impact, Notched (ISO) 5.70 kJ/m²
2.71 ft-lb/in²
ISO 180-A
Processing Properties Metric English Comments
Melt Temperature 230 - 250 °C
446 - 482 °F
Mold Temperature 65.0 - 80.0 °C
149 - 176 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 - 6 hour
4 - 6 hour
Moisture Content <= 0.20 %
<= 0.20 %