Polymer Property : Puncture Energy = 22.9 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 31.0 - 31.0 J

@Temperature -30.0 - -30.0 °C
22.9 - 22.9 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 31.0 J Grade Count:1
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..