Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 31.0 - 31.0 J @Temperature -30.0 - -30.0 °C |
22.9 - 22.9 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 31.0 J Grade Count:1 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |