Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 31.0 - 31.0 J @Temperature -30.0 - -30.0 °C |
22.9 - 22.9 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 31.0 J Grade Count:1 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Puncture Energy | 31.0 J | 22.9 ft-lb | Puncture Resistance @Max Load, 23°C; ASTM D3763 |
Eastman Drystar 0827 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Puncture Energy | 31.0 J | 22.9 ft-lb | Puncture Resistance @Max Load, 23°C; ASTM D3763 |
Eastman Eastar EN076 Copolyester Eastar Copolyester EN076 is recommended for the thick-walled containers that are prevalent in the cosmetics and personal care markets. This copolyester offers good processability with the benefits o.. |