Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 4.50 J @Temperature -30.0 °C |
3.32 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® BKV 215 H2.0 901510 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 115, conditioning .. |
|||
Puncture Energy | 4.50 J @Temperature -30.0 °C |
3.32 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® BKV 215 H2.0 901510 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 115, conditioning .. |
|||
Puncture Energy | 4.50 J | 3.32 ft-lb | Dynatup; ASTM D3763 |
Eastman Tritan FX200 Copolyester Eastman Tritan FX200 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w.. |
|||
Puncture Energy | 4.50 J @Load 98.9 kg |
3.32 ft-lb @Load 218 lb |
DAM; ISO 6603-2 |
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |