Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.000620 GPa @Temperature 815 °C |
0.0899 ksi @Temperature 1500 °F |
ASTM C258 |
BNZ Materials Bazelite 2000 Insulating Castable BNZ manufactures a variety of insulating and dense castable refractories to meet the exacting needs of the high temperature processing industries. These hydraulic setting products are suitable for i.. |
|||
Modulus of Rupture | 0.000620 GPa @Temperature 1095 °C |
0.0899 ksi @Temperature 2003 °F |
ASTM C258 |
BNZ Materials Bazelite 2000 Insulating Castable BNZ manufactures a variety of insulating and dense castable refractories to meet the exacting needs of the high temperature processing industries. These hydraulic setting products are suitable for i.. |
|||
Modulus of Rupture | 0.000620 GPa @Temperature 1095 °C |
0.0899 ksi @Temperature 2003 °F |
ASTM C268 |
BNZ Materials Bazelite 2300 Insulating Castable Blaz 2300 is a lightweight, general purpose insulating castable. Can be used for back-up or exposed to furnace conditions. Used for one-shot linings, petrochemical heaters, combustion chambers and f.. |
|||
Modulus of Rupture | 0.000620 GPa @Temperature 1260 °C |
0.0899 ksi @Temperature 2300 °F |
ASTM C268 |
BNZ Materials Bazelite 2300 LI Insulating Castable Blaz 2300 L is similar to Blaz 2300 but suitable for those applications where reducing conditions might be encountered. These high purity, low iron products are specifically designed for both back-u.. |
|||
Modulus of Rupture | 0.000620 GPa @Temperature 815 °C |
0.0899 ksi @Temperature 1500 °F |
ASTM C268 |
BNZ Materials Bazelite 2300 VLI Insulating Castable Blaz 2300 VLI is similar to Blaz 2300 but suitable for those applications where reducing conditions might be encountered. These high purity, low iron products are specifically designed for both back.. |
|||
Modulus of Rupture | 0.000620 GPa @Temperature 1095 °C |
0.0899 ksi @Temperature 2003 °F |
ASTM C268 |
BNZ Materials Bazelite 2300 VLI Insulating Castable Blaz 2300 VLI is similar to Blaz 2300 but suitable for those applications where reducing conditions might be encountered. These high purity, low iron products are specifically designed for both back.. |