Mechanical Properties Metric English Comments
Modulus of Rupture 1.92e-7 - 0.00118 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000279 - 0.171 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories GUN-100L Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 1.92e-7 - 0.00118 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000279 - 0.171 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories GUN-110L Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 1.92e-7 - 0.00118 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000279 - 0.171 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories GUN-120L Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).