Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 1.92e-7 - 0.00118 GPa @Temperature 110 °C, Time 86400 sec |
0.0000279 - 0.171 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories GUN-100L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 1.92e-7 - 0.00118 GPa @Temperature 110 °C, Time 86400 sec |
0.0000279 - 0.171 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories GUN-110L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 1.92e-7 - 0.00118 GPa @Temperature 110 °C, Time 86400 sec |
0.0000279 - 0.171 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories GUN-120L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |