Mechanical Properties Metric English Comments
Tear Strength 19.1 kN/m
109 pli
Die B, Fluorosilicone Property; ASTM D624
Arlon R37503G015 0.015" (0.381 mm) Cured Fluorosilicone Rubber
Design/Construction: Interleave: PolyethyleneSide 2: Cured Fluorosilicone RubberSubstrate: Polyester FabricSide 2: Cured Fluorosilicone Rubber Substrate Weave: PlainFabric Count (Wrap x Fill): 88 x ..