Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 19.1 kN/m | 109 pli | Die B, Fluorosilicone Property; ASTM D624 |
Arlon R37503G015 0.015" (0.381 mm) Cured Fluorosilicone Rubber Design/Construction: Interleave: PolyethyleneSide 2: Cured Fluorosilicone RubberSubstrate: Polyester FabricSide 2: Cured Fluorosilicone Rubber Substrate Weave: PlainFabric Count (Wrap x Fill): 88 x .. |