Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase TPSiV® 4000-50A Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV) , Silicone, Thermoplastic
Manufacturer Multibase
Trade Name TPSiV®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase TPSiV® 4000-50A Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mobile communication devices, computers, and sport &leisure applications.Information provided by Multibase, a Dow Corning Company
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ISO 1183
Linear Mold Shrinkage 0.020 - 0.040 cm/cm
0.020 - 0.040 in/in
Melt Flow 55 g/10 min

@Load 10.0 kg,
Temperature 190 °C
55 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 48
48
ISO 868
Tensile Strength 4.40 MPa
638 psi
ISO 37
Tensile Strength, Ultimate 1.50 MPa
218 psi
ISO 37
Elongation at Break 710 %
710 %
ISO 37
Flexural Strength 0.740 MPa
107 psi
ISO 178
Flexural Modulus 0.0140 GPa
2.03 ksi
ISO 178
Tear Strength 20.1 kN/m
115 pli
ISO 34
Taber Abrasion, mg/1000 Cycles 155
155
ASTM D3389
Compression Set 25 %

@Temperature 23.0 °C,
Time 79200 sec
25 %

@Temperature 73.4 °F,
Time 22.0 hour
ISO 815
77 %

@Temperature 70.0 °C,
Time 79200 sec
77 %

@Temperature 158 °F,
Time 22.0 hour
ISO 815
Processing Properties Metric English Comments
Feed Temperature 150 - 160 °C
302 - 320 °F
Middle Barrel Temperature 155 - 165 °C
311 - 329 °F
Front Barrel Temperature 160 - 170 °C
320 - 338 °F
Nozzle Temperature 170 - 190 °C
338 - 374 °F
Melt Temperature 180 °C
356 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Drying Temperature 65.0 - 80.0 °C
149 - 176 °F
Dry Time 2 - 4 hour
2 - 4 hour
Descriptive Properties Value Comments
Injection Speed MED-FAST