PolyOne OnFlex™ HFFR 320-01 Thermoplastic Elastomer (TPE)

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer PolyOne Corporation
Trade Name OnFlex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne OnFlex™ HFFR 320-01 Thermoplastic Elastomer (TPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OnFlex™ HFFR 320-01 is a non-halogen flame retardant material designed for flexible power cord insulation and cable jackets. New Product. Commercial specifications have not been established. - Non-halogen flame retardant - UL62 compliantPurge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP).Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
ASTM D792
Viscosity 35000 cP

@Shear Rate 11200 1/s,
Temperature 200 °C
35000 cP

@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
1.25e+6 cP

@Shear Rate 67.0 1/s,
Temperature 200 °C
1.25e+6 cP

@Shear Rate 67.0 1/s,
Temperature 392 °F
ASTM D3835
Maximum Moisture Content 0.020
0.020
Deformation 35 %

@Temperature 150 °C
35 %

@Temperature 302 °F
300g; UL 1581
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
10 sec; ASTM D2240
Tensile Strength at Break 20.7 MPa
3000 psi
UL 1581
15.2 MPa

@Temperature 23.0 °C
2200 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 260 %
260 %
UL 1581
240 %

@Temperature 23.0 °C
240 %

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tear Strength 49.1 kN/m
280 pli
ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
UL Temperature Rating; UL 1581
Brittleness Temperature -40.0 °C
-40.0 °F
ASTM D746
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
All Color; UL 94
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
All Color; UL 94
Oxygen Index 27 %
27 %
ASTM D2863-08
Electrical Properties Metric English Comments
Volume Resistivity 2.90e+15 ohm-cm

@Temperature 23.0 °C
2.90e+15 ohm-cm

@Temperature 73.4 °F
50% RH, ASTM D257-07; ASTM D257
Dielectric Strength 50.0 kV/mm

@Thickness 0.533 mm,
Temperature 23.0 °C
1270 kV/in

@Thickness 0.0210 in,
Temperature 73.4 °F
50% RH, ASTM D149-97a(04); ASTM D149
Processing Properties Metric English Comments
Zone 1 180 - 190 °C
356 - 374 °F
Zone 2 200 - 210 °C
392 - 410 °F
Zone 3 210 - 220 °C
410 - 428 °F
Zone 4 210 - 220 °C
410 - 428 °F
Die Temperature 210 - 220 °C
410 - 428 °F
Drying Temperature 70.0 °C
158 °F
Dry Time 2.00 - 3.00 hour
2.00 - 3.00 hour
Descriptive Properties Value Comments
Agency Ratings UL 94 .QMFZ2.E76261
Aging Resistance 100%
UL 1581; 136°C; Thermal aging tensile retention 168hrs.
85%
UL 1581; 136°C; Thermal aging elongation retension168hrs.
Appearance Black
Green
Natural Color
White
Features Flame Retardant
Forms Pellets
Generic Material TPE
Generic Name Thermoplastic Elastomer (TPE)
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Cable Jacketing
Flexible Cord Insulation
VW-1 pass
UL 1581