Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 29.6 kN/m
169 pli
ISO 34/1
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell..
Tear Strength 29.6 kN/m
169 pli
ISO 34/1
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell..
Tear Strength 29.6 kN/m
169 pli
ISO 34/1
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell..
Tear Strength 29.6 kN/m
169 pli
ISO 34/1
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and exc..
Tear Strength 29.6 kN/m
169 pli
ISO 34/1
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell..
Tear Strength 29.6 kN/m
169 pli
ISO 34/1
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and exc..
Tear Strength 29.6 kN/m
169 pli
ISO 34/1
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell..
Tear Strength 29.6 kN/m
169 pli
ISO 34/1
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and exc..
Tear Strength 29.6 kN/m
169 pli
ISO 34/1
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5070UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell..
Tear Strength 29.6 kN/m
169 pli
ISO 34/1
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and exc..
Tear Strength 29.6 kN/m
169 pli
ISO 34/1
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and exc..
Tear Strength 29.6 kN/m
169 pli
Die C, Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4640 Low Cost General Purpose Hose
FormulationNordel® IP 4640
Tear Strength 29.6 kN/m
169 pli
ISO 34/1
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and exc..