Mechanical Properties Metric English Comments
Tear Strength 53.8 kN/m
307 pli
ASTM D624
Multibase Multi-Flex® TPE G 7455 X
Multi-Flex® G 7455 X is based on the Kraton G 78455 X formulation. It has low specific gravity as well as having a UL 94 rating of V-0. Ash is 5.2%. Multi-Flex TPE contains Kraton™ G.Data provi..
Tear Strength 53.8 kN/m
307 pli
Die C
NEU NeuSoft™ 602-60A Ester TPU / SBC blend
Tear Strength 53.8 kN/m
307 pli
Die 'C' Tear; 20 in/min; ASTM D624
PolyOne Elastamax XL 1092-2 TPU-Based Thermoplastic Elastomer  (discontinued **)