Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 53.8 kN/m | 307 pli | ASTM D624 |
Multibase Multi-Flex® TPE G 7455 X Multi-Flex® G 7455 X is based on the Kraton G 78455 X formulation. It has low specific gravity as well as having a UL 94 rating of V-0. Ash is 5.2%. Multi-Flex TPE contains Kraton™ G.Data provi.. |
|||
Tear Strength | 53.8 kN/m | 307 pli | Die C |
NEU NeuSoft™ 602-60A Ester TPU / SBC blend |
|||
Tear Strength | 53.8 kN/m | 307 pli | Die 'C' Tear; 20 in/min; ASTM D624 |
PolyOne Elastamax XL 1092-2 TPU-Based Thermoplastic Elastomer
(discontinued **) This is a general purpose thermoplastic elastomer based on modified TPU technology. Physical Form: Pellet. Standard Color: Natural.Information provided by M. A. Hanna. M. A. Hanna and Geon merged.. |