Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 61.3 kN/m | 350 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Wire & Cable JA612EA Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 61.4 kN/m | 350 pli | Split; ASTM D624 |
Northstar Polymers MSS-A80AQ High Performance Polyurethane Cast Elastomer System 80A This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio.. |
|||
Tear Strength | 61.3 kN/m | 350 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible 86479 Opaque Polyvinyl Chloride Information provided by PolyOne |
|||
Tear Strength | 61.3 kN/m | 350 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 61.3 kN/m | 350 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 6.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 61.4 kN/m | 350 pli | 25 mil film; ASTM D624 |
Huntsman IROGRAN® A 85 P 4394 UV TPU-Polyether Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS.. |
|||
Tear Strength | 61.4 kN/m | 350 pli | ASTM D624 |
Huntsman IROGRAN® PS455-203 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Tear Strength | 61.4 kN/m | 350 pli | Die C; ASTM D624 |
Mearthane Durethaneâ„¢ S DS-370A Solid Polyurethane Elastomer TDI backbone: ether.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
Tear Strength | 61.4 kN/m | 350 pli | ASTM D624 |
Multibase Multi-Flex® G 7827 Black TPE Styrene Ethylene Butylene Styrene Block Copolymer Forms: PelletsProcessing Methods:Injection Molding Uses: Automotive ApplicationsInformation provided by Multibase |
|||
Tear Strength | 61.4 kN/m | 350 pli | Die C; ASTM D624 |
Mearthane Durethaneâ„¢ S DS-390A Solid Polyurethane Elastomer TDI backbone: ether.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
Tear Strength | 61.4 kN/m | 350 pli | Warp/Longitudinal direction; ASTM D1000 |
Saint-Gobain COHRlastic® 1025 General-Purpose Electrical-Grade Silicone Coated Fabric Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi.. |
|||
Tear Strength | 61.4 kN/m | 350 pli | Warp/Longitudinal direction; ASTM D1000 |
Saint-Gobain COHRlastic® 3016 Low Temperature Flexibility Silicone Coated Fabric Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi.. |
|||
Tear Strength | 61.4 kN/m | 350 pli | Fill/Transverse direction |
Saint-Gobain COHRlastic® 3032 Low Temperature Flexibility Silicone Coated Fabric Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi.. |
|||
Tear Strength | 61.4 kN/m | 350 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® TCK® 1589 High-Strength Plain Weave Open Mesh Belting Material Description: General Notes on Saint Gobain Chemfab® TCK® Open Mesh Belting Products:TCK belting products are PTFE (PTFE = polytetrafluoroethylene) coated Kevlar®, a high-temperature aramid .. |
|||
Tear Strength | 61.4 kN/m | 350 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® TCK® 1589 High-Strength Plain Weave Open Mesh Belting Material Description: General Notes on Saint Gobain Chemfab® TCK® Open Mesh Belting Products:TCK belting products are PTFE (PTFE = polytetrafluoroethylene) coated Kevlar®, a high-temperature aramid .. |
|||
Tear Strength | 61.4 kN/m | 350 pli | Initial Tear Strength; ASTM D1004-93 |
Saint-Gobain Tygothane® C-544-AI.B. Precision Polyurethane Pressure Tubing Formulation Description: Tygothane® C-544-A I.B.: More flexible than many other reinforced urethane tubings, Tygothane® Pressure Tubing can be used in some of the most physically demanding applications,.. |
|||
Tear Strength | 61.4 kN/m | 350 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 1580 PTFE Coated Fiberglass Conveyor Belting Description: General Notes on Saint Gobain Open Mesh Belting Products:CHEMFAB 1580, 1589 and 1590 are woven fiberglass belting materials designed for use in forced hot air curing ovens. Saint-Gobain.. |
|||
Tear Strength | 61.4 kN/m | 350 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® TCKGN Heavyweight Rough Surface Belting Description: General Notes on Saint Gobain Belting Products:Saint Gobain Performance Plastics developed its belting materials for applications that require superior release characteristics, permeabi.. |
|||
Tear Strength | 61.4 kN/m | 350 pli | Die C; ASTM D1004 |
Teknor Apex TEKRON® 4300-D88A Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tear Strength | 61.3 kN/m | 350 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 70A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 61.3 kN/m | 350 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 82A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 61.3 kN/m | 350 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 61.3 kN/m | 350 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.5 PHR Sulfur Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |
|||
Tear Strength | 61.3 kN/m | 350 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 4.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 61.3 kN/m | 350 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 82A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 61.3 kN/m | 350 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.5 PHR Sulfur Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |
|||
Tear Strength | 61.3 kN/m | 350 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 6.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 61.4 kN/m | 350 pli | ASTM D412 |
ACC ReactAmine® EP 350 EPI Engineered Polymers Polyurea ReactAmine® EP-350 is a two component 100% solid Polyurea with superior performance in industrial applications. EP-350 displays extremely fast cure times with excellent adhesions to different subst.. |