Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 17.0 kN/m | 97.0 pli | Die B |
Momentive Performance Materials Silplusâ„¢ 40 MP Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 4002 DARK GRAY Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | ISO 34B |
Huntsman AVALON® 650 B Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | ISO 6383 |
SABIC Innovative Plastics NORYL WCP821 PPE-TPE Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain .. |
|||
Tear Strength | >= 17.0 kN/m | >= 97.0 pli | |
Silikony Polskie Polsil Gum 100/50 HTV Silicone Rubber Polsil Gum is a general purpose master batch compound, vulcanizing at high temperature after addition of vulcanizing agent. Silicone rubber obtained from Polsil® GUM shows useful properties: agei.. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | |
Trelleborg B702 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | |
Trelleborg S550 Silicone Rubber PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering... |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | |
Trelleborg S561 Silicone Rubber PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering... |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | |
Trelleborg S665 Silicone Rubber PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering... |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | |
Dow Corning HV 1650/50 SILICONE RUBBER 50 Shore A hardness high consistency silicone rubber with excellent tracking and erosion resistance and low modulusInformation provided by Dow Corning |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | |
Dow Corning HV 1760/65 Silicone Rubber 65 Shore hardness high consistency silicone rubber with fast cure system and excellent tracking and erosion resistanceInformation provided by Dow Corning |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | ASTM D624 |
ELASTO UK Dryflex® 502350S SEBS Based Material, Unfilled Qualities, 35A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | {ppiw], Die B, Silicone Property; ASTM D624 |
Arlon 55629R028 0.0285" (0.724 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Appearance: Red silicone gum on fiberglassThis data repre.. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | Silicone Property; ASTM D624 |
Arlon 56606R026 0.027" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production materia.. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon P30670R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone Rubber Substrate: Style 1165 FiberglassAppearance: Red silicone gum on fiberglass with polymer release linersThis data represents typical values for the.. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | ASTM D 624 |
API Megol AM DP2392/32 SEBS Adhesion Modified Overmolding for Polar Polymers Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
Tear Strength | >= 17.0 kN/m | >= 97.0 pli | |
Silikony Polskie Polsil Gum 213/60 HTV Silicone Rubber Polsil Gum is a general purpose master batch compound, vulcanizing at high temperature after addition of vulcanizing agent. Silicone rubber obtained from Polsil® GUM shows useful properties: ageing.. |