Mechanical Properties Metric English Comments
Flexural Strength 280 MPa

@Temperature 23.0 °C
40600 psi

@Temperature 73.4 °F
ISO 178
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced
Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo..
Flexural Strength 280 MPa

@Temperature 23.0 °C
40600 psi

@Temperature 73.4 °F
ISO 178
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c..
Flexural Strength 280 MPa

@Strain 4.20 %
40600 psi

@Strain 4.20 %
ISO 178
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers
PA 66, 30% glass fibers, injection molding, heat-ageing stabilized
Flexural Strength 280 MPa

@Temperature 23.0 °C
40600 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-663G30 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 280 MPa

@Temperature 23.0 °C
40600 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 1.0%); ASTM-D790
Toyobo GLAMIDE® TY-791GT 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 280 MPa

@Temperature -40.0 °C
40600 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 1.4%); ASTM-D790
Toyobo GLAMIDE® TY-791HT 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 280 MPa

@Treatment Temp. 100 °C,
Time 3600 sec
40600 psi

@Treatment Temp. 212 °F,
Time 1.00 hour
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Description: Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. UL-94 V..
Flexural Strength 280 MPa

@Thickness >=1.50 mm
40600 psi

@Thickness >=0.0591 in
1hr/150°C/measured at 150°C; ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax EP 203 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Description: High mechanical strength at elevated temperatures. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. Can be used at c..