Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 26.2 MPa @Temperature 260 °C |
3800 psi @Temperature 500 °F |
ASTM D732 |
Greene Tweed Arlon® 2000 Polyketone Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
Shear Strength | 26.20 MPa @Temperature 121 °C |
3800 psi @Temperature 250 °F |
90 min @ 350°F, Spring Clamp Pressure, FPL Acid Etched 6061-T6; ASTM D1002 |
Zyvex Performance Materials Aroply™ 350 Nano-Engineered Composite Film Adhesive Aroply™ 350 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported carrier. Cured adhesive character.. |
|||
Shear Strength | 26.2 MPa @Temperature 71.0 °C |
3800 psi @Temperature 160 °F |
Short Beam, Wet (14 ± 1/2 days of water immersion at 160 ± 5°F (71 ± 3°C) |
Hexcel® HexPly® F522 Epoxy Resin, W3C282 Carbon Fabric Hexcel designation: TW3C282-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel |
|||
Shear Strength | 26.2 MPa @Temperature 21.1 °C |
3800 psi @Temperature 70.0 °F |
Lap Shear |
Hexcel® Redux® 335K Adhesive film for bonding metallic and composite components (0.03 psf) Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for a.. |
|||
Shear Strength | 26.2 MPa @Temperature 71.0 °C |
3800 psi @Temperature 160 °F |
Short Beam, Wet (14 ± 1/2 days of water immersion at 160 ± 5°F (71 ± 3°C) |
Hexcel® HexPly® F522 Epoxy Resin, F3C433 Carbon Fabric Hexcel designation: F3C433-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel |