Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 36.0 MPa @Temperature 90.0 °C |
5220 psi @Temperature 194 °F |
0°, Interlaminar, Conditioning: 23°C; ASTM D2344 |
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, 3K High Strength Carbon Fiber Designation: C280T4; Twill 4x4Information provided by HexCel |
|||
Shear Strength | 36.0 MPa @Temperature 22.2 °C |
5220 psi @Temperature 72.0 °F |
Lap Shear, Primed with Redux 119 |
Hexcel® Redux® 319A High Performance Modified Epoxy Film Adhesive (0.06 psf) Redux 319 is a high performance modified epoxy film adhesive curing at 350°F. It is available in both supported and unsupported versions at areal weights between 0.03 and 0.08 psf. The supported ve.. |
|||
Shear Strength | 36.0 MPa @Temperature 24.0 °C |
5220 psi @Temperature 75.2 °F |
Short Beam |
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric Hexcel designation: 120-38"-F161; Fiber: Kev. 49 195Information provided by HexCel |
|||
Shear Strength | 36.0 MPa @Temperature 90.0 °C |
5220 psi @Temperature 194 °F |
0°, Interlaminar, Conditioning: 23°C; ASTM D2344 |
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, 6K High Strength Carbon Fiber Designation: C370S5, Satin weave, 5HInformation provided by HexCel |