Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 69.0 MPa @Temperature 23.0 °C |
10000 psi @Temperature 73.4 °F |
0°, Interlaminar, Conditioning: 23°C; ASTM D2344 |
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, 6K High Strength Carbon Fiber Designation: C370S5, Satin weave, 5HInformation provided by HexCel |