Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 7.93 MPa @Temperature 82.0 °C |
1150 psi @Temperature 180 °F |
Overlap, FRP |
3M Scotch-Weld™ TE100 Black Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Shear Strength | 7.93 MPa @Temperature 23.0 °C |
1150 psi @Temperature 73.4 °F |
Overlap, Polyacrylic, Substrate Failure |
3M Scotch-Weld™ TE100 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Shear Strength | 7.93 MPa @Time 605000 sec |
1150 psi @Time 168 hour |
Overlap, Maple |
3M Scotch-Weld™ EZ250150 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th.. |
|||
Shear Strength | 7.93 MPa @Temperature 23.0 °C |
1150 psi @Temperature 73.4 °F |
Overlap, Polyacrylic |
3M Scotch-Weld™ TS115 HGS Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Shear Strength | 7.93 MPa @Temperature 24.0 °C |
1150 psi @Temperature 75.2 °F |
Overlap, FRP, Substrate Failure |
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 7.93 MPa @Temperature 24.0 °C |
1150 psi @Temperature 75.2 °F |
Overlap, FRP, Substrate Failure |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 7.93 MPa @Temperature 24.0 °C |
1150 psi @Temperature 75.2 °F |
Overlap, FRP, Substrate Failure |
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 7.93 MPa @Temperature 23.0 °C |
1150 psi @Temperature 73.4 °F |
Overlap, Polyacrylic, Substrate Failure |
3M Scotch-Weld™ TE015 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Shear Strength | 7.93 MPa @Temperature 23.0 °C |
1150 psi @Temperature 73.4 °F |
Overlap, PVC, Substrate Failure |