Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 71.0 MPa @Temperature 21.1 °C |
10300 psi @Temperature 70.0 °F |
Short-Beam, Dry; Autoclave Cured; ASTM D2344 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 6K 4HS IM7 Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Shear Strength | 71.0 MPa @Temperature 50.0 °C |
10300 psi @Temperature 122 °F |
ILSS Weft; 10 min @ 250°F |
Hexcel® HexPly® EF01 Epoxy Curing System after THR 120 EF01 S25 38% Curing Cycle Information provided by HexCel |
|||
Shear Strength | 71.0 MPa @Temperature 50.0 °C |
10300 psi @Temperature 122 °F |
ILSS Weft; 15 min @ 250°F |
Hexcel® HexPly® EF01 Epoxy Curing System after THR 120 EF01 S25 38% Curing Cycle Information provided by HexCel |
|||
Shear Strength | 71.0 MPa @Temperature 50.0 °C |
10300 psi @Temperature 122 °F |
ILSS Weft; 30 min @ 250°F |
Hexcel® HexPly® EF01 Epoxy Curing System after THR 120 EF01 S25 38% Curing Cycle Information provided by HexCel |
|||
Shear Strength | 71.0 MPa @Temperature 23.0 °C |
10300 psi @Temperature 73.4 °F |
ILSS; prEN2563 |
Hexcel® HexPly® M35-4 80-180°C Curing Epoxy Matrix, M35-4/40%/G1089/1000 Fabric Fiber: T800H 6K 2x2 Twill, 200 g/m2Information provided by HexCel |