Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 61.0 MPa @Temperature 24.0 °C |
8850 psi @Temperature 75.2 °F |
Short Beam, Dry |
Hexcel® HexPly® F522 Epoxy Resin, W3C282 Carbon Fabric Hexcel designation: TW3C282-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel |
|||
Shear Strength | 61.0 MPa @Temperature 100 °C |
8850 psi @Temperature 212 °F |
ILSS; prEN2563 |
Hexcel® HexPly® M35-4 80-180°C Curing Epoxy Matrix, M35-4/40%/G1089/1000 Fabric Fiber: T800H 6K 2x2 Twill, 200 g/m2Information provided by HexCel |
|||
Shear Strength | 61.0 MPa @Temperature 80.0 °C |
8850 psi @Temperature 176 °F |
ILSS; prEN2563 |
Hexcel® HexPly® M35-4 80-180°C Curing Epoxy Matrix, M35-4/40%/G803/1200 Fabric Fiber: T300 3K, 285 g/m2Information provided by HexCel |