Mechanical Properties Metric English Comments
Shear Modulus 0.775 GPa

@Temperature 100 °C
112 ksi

@Temperature 212 °F
ISO 6721
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone
Description: Medium viscosity injection-molding and extrusion grade with good toughness and chemical resistance (stress crack resistance), resistant against superheated steam. The property profile m..