Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.775 GPa @Temperature 100 °C |
112 ksi @Temperature 212 °F |
ISO 6721 |
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone Description: Medium viscosity injection-molding and extrusion grade with good toughness and chemical resistance (stress crack resistance), resistant against superheated steam. The property profile m.. |