Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Vicat Softening Point = 109 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 109 - 109 °C

@Temperature 120 - 120 °C
228 - 228 °F

@Temperature 248 - 248 °F
Average value: 109 °C Grade Count:2
Overview of materials for Polystyrene, Heat Resistant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values..
Vicat Softening Point 109 - 109 °C

@Load 1.02 - 1.02 kg
228 - 228 °F

@Load 2.25 - 2.25 lb
Average value: 109 °C Grade Count:2
Overview of materials for Polystyrene, Heat Resistant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values..
Vicat Softening Point 76.0 - 109 °C
169 - 228 °F
Average value: 99.0 °C Grade Count:28
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..