Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 76.0 °C | 169 °F | 5kg load; ISO 306 |
Eastman Eastar GN002 Copolyester, Natural
(discontinued **) Eastar GN002 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN002 copolyester will not crystallize and thus offers wider processing latitude tha.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | 5kg load; ISO 306 |
Eastman Eastar GN005 Copolyester, Natural
(discontinued **) Eastar GN005 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN005 copolyester will not crystallize and thus offers wider processing latitude tha.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | |
Eastman Eastapak 9921W PET
(discontinued **) Unreinforced. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | Softening Point, R&B; ASTM E-28 |
ExxonMobil Escorene® MV-02528 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 27.5% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | VST/B/50; ISO 306 |
GEHR Plastics PE-UHMW-ELS Polyethylene
(discontinued **) Polyethylene offers resistance to almost all acids and bases, detergents and hot water. PE has good insulation properties and is easy to weld. The operating temperature of HDPE is from -58 °F to +1.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | ASTM D1525 |
Huntsman PE1903 EVA Film Extrusion
(discontinued **) 9% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent toughness and flexibility at low temperatures, and good heat-seal response.Applications: Film extrusion: laminating film, controll.. |
|||
Vicat Softening Point | 76.0 - 154 °C | 169 - 309 °F | Average value: 122 °C Grade Count:11 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Vicat Softening Point | 76.0 - 270 °C | 169 - 518 °F | Average value: 92.7 °C Grade Count:16 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Vicat Softening Point | 76.0 - 78.0 °C @Load 5.00 kg |
169 - 172 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RKT 736/K1 Rigid PVC, Extrusion Lead Free Transparent profiles |
|||
Vicat Softening Point | 76.0 °C | 169 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Europe-Africa-Middle East) Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | ISO 306 |
Stir SpA Giesse RSA/12 (PVC) Application: Blow molding very high shock resistanceInformation provided by STIR SpA |
|||
Vicat Softening Point | 76.0 °C | 169 °F | ISO 306 |
Stir SpA Giesse RSA/8 (PVC) Application: Blow molding medium shock resistanceInformation provided by STIR SpA |
|||
Vicat Softening Point | 76.0 °C | 169 °F | VST/A/50; ISO 306 |
Styrolution Styrolux® 693 D SBC Description: Styrolux® 693 D is a clear styrene-butadiene copolymer (SBC) with a well balanced combination of toughness and clarity. Styrolux® 693 D is mainly used for thermoformed articles, e.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | ASTM D1525 |
Westlake EB502 12.5% EVA Copolymer Westlake Elevate™ EB502 resin is a fractional melt index 12.5% VA ethylene vinyl acetate copolymer designed for flexible packaging and other films that require excellent toughness and good heat sea.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | 5kg load; ISO 306 |
Eastman Drystar 0113 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | |
Eastman Eastapak 9921 PET ISO data as provided by the manufacturer, Eastman Chemical |
|||
Vicat Softening Point | 76.0 °C | 169 °F | ASTM D1525 |
Chevron Phillips K-Resin® KK38 Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene CopolymerCustomer Benefits: KK38 is an improved extrusion grade SBC designed specifically for superior performance in blends with general purpose polystyrene. It is easily process.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | ASTM D-1525 |
Chevron Phillips K-Resin® XK44 SBC K-Resin® Styrene-Butadiene Copolymer (SBC)Applications:Thermoformed clam shell packagingThermoformed blister packsThermoformed medical traysBlow molded productsFeatures:Good clarityGood stiffnessGo.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | ASTM D1525 |
Dow AFFINITY™ PF 1146G Polyolefin Plastomer (POP) AFFINITY™ PF 1140G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for high speed packaging applications requiring low seal initiation temperature and good machina.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | |
Dow Primacor® 2912 Ethylene Acrylic Acid (EAA) PRIMACOR® 2912 polymer containing 9.5% comonomer is an extrusion/ coextrusion coating resin for flexible packaging applications. It is designed to provide excellent adhesion to metallic, paper and .. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | ASTM D1525 |
Dow Engage® 8440 Polyolefin Elastomer Description: Engage® 8440 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It is an excellent thermoplastic elastomer .. |
|||
Vicat Softening Point | 76.0 - 78.0 °C @Load 5.00 kg |
169 - 172 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds ARC 10 Rigid PVC, Atoxic for General Purpose Bottles medium antishock |
|||
Vicat Softening Point | 76.0 °C @Load 0.999 kg |
169 °F @Load 2.20 lb |
ASTM D1525 |
Arkema Group LOTADER® 3210 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 3210 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. Main applicationsLOTADER 3210 is a versatile adhesive for extrusi.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | 49 N; ISO 306 |
A.D. Compound Adene NCQAG Copolymer 40% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Vicat Softening Point | 76.0 °C | 169 °F | 50°C/hr; 50N |
Arkema Group Kynar® FLEX 2821 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EDN, N. ?E5.C.H.B.C,, ? (2.5-6.5)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousn.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | 50°C/hr; 50N |
Arkema Group Kynar® FLEX 2822 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EDN, N. ?E5.C.H.B.C,, ? (4-8)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousness .. |
|||
Vicat Softening Point | 76.0 - 78.0 °C @Load 5.00 kg |
169 - 172 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RKT 736 Rigid PVC, Extrusion Lead Free Transparent antishock profiles |
|||
Vicat Softening Point | 76.0 °C | 169 °F | ASTM D1525 |
C.O.I.M. LARIPUR® LPR7015 Plasticized Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | ISO 306B |
Lucite International Elvakon® 4451 Super Low Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable prot.. |