Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 76.0 °C | 169 °F | 5kg load; ISO 306 |
Eastman Eastar GN002 Copolyester, Natural
(discontinued **) Eastar GN002 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN002 copolyester will not crystallize and thus offers wider processing latitude tha.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | 5kg load; ISO 306 |
Eastman Eastar GN005 Copolyester, Natural
(discontinued **) Eastar GN005 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN005 copolyester will not crystallize and thus offers wider processing latitude tha.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | |
Eastman Eastapak 9921W PET
(discontinued **) Unreinforced. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003. |
|||
Vicat Softening Point | 76.1 °C | 169 °F | ASTM D1525 |
ExxonMobil LD 509.48 Compounding Resin
(discontinued **) LD 509.48 is a high melt index homopolymer resin designed to provide good processability in compounding applications.Information provided by ExxonMobil Chemical |
|||
Vicat Softening Point | 76.0 °C | 169 °F | VST/B/50; ISO 306 |
GEHR Plastics PE-UHMW-ELS Polyethylene
(discontinued **) Polyethylene offers resistance to almost all acids and bases, detergents and hot water. PE has good insulation properties and is easy to weld. The operating temperature of HDPE is from -58 °F to +1.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | ASTM D1525 |
Huntsman PE1903 EVA Film Extrusion
(discontinued **) 9% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent toughness and flexibility at low temperatures, and good heat-seal response.Applications: Film extrusion: laminating film, controll.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Europe-Africa-Middle East) Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | ISO 306 |
Stir SpA Giesse RSA/8 (PVC) Application: Blow molding medium shock resistanceInformation provided by STIR SpA |
|||
Vicat Softening Point | 76.0 °C | 169 °F | VST/A/50; ISO 306 |
Styrolution Styrolux® 693 D SBC Description: Styrolux® 693 D is a clear styrene-butadiene copolymer (SBC) with a well balanced combination of toughness and clarity. Styrolux® 693 D is mainly used for thermoformed articles, e.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Asia Pacific) Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | ASTM D1525 |
DuPont Elvax® 3130 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film 12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | ASTM D1525 |
Chevron Phillips K-Resin® KK38 Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene CopolymerCustomer Benefits: KK38 is an improved extrusion grade SBC designed specifically for superior performance in blends with general purpose polystyrene. It is easily process.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | ASTM D-1525 |
Chevron Phillips K-Resin® XK44 SBC K-Resin® Styrene-Butadiene Copolymer (SBC)Applications:Thermoformed clam shell packagingThermoformed blister packsThermoformed medical traysBlow molded productsFeatures:Good clarityGood stiffnessGo.. |
|||
Vicat Softening Point | 76.1 °C | 169 °F | ASTM D1525 |
ExxonMobil Escorene™ FL 00014 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00014 is a copolymer of ethylene and vinyl acetate. For film requiring very high toughness, low creep, excellent optical properties and low gel.Availability: Africa & Middle .. |
|||
Vicat Softening Point | 76.1 °C | 169 °F | ASTM D1525 |
ExxonMobil Exact™ 4151 Ethylene-based Plastomer Resin Product Description: Exact 4151 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4151 is designed for both monolayer and multilayer coe.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | ASTM D1525 |
Dow AFFINITY™ PF 1146G Polyolefin Plastomer (POP) AFFINITY™ PF 1140G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for high speed packaging applications requiring low seal initiation temperature and good machina.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | |
Dow Primacor® 2912 Ethylene Acrylic Acid (EAA) PRIMACOR® 2912 polymer containing 9.5% comonomer is an extrusion/ coextrusion coating resin for flexible packaging applications. It is designed to provide excellent adhesion to metallic, paper and .. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | ASTM D1525 |
Dow Engage® 8440 Polyolefin Elastomer Description: Engage® 8440 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It is an excellent thermoplastic elastomer .. |
|||
Vicat Softening Point | 76.1 °C | 169 °F | |
Dow Primacor® 3440 Ethylene Acrylic Acid (EAA) PRIMACOR® 3440 polymer containing 9.5% comonomer is an extrusion/ coextrusion coating and laminating for flexible packaging applications. It is designed to provide excellent hot tack and adhesion t.. |
|||
Vicat Softening Point | 76.0 - 78.0 °C @Load 5.00 kg |
169 - 172 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds ART 10 Rigid PVC, Atoxic for General Purpose Transparent bottles medium antishock |
|||
Vicat Softening Point | 76.0 °C @Load 0.999 kg |
169 °F @Load 2.20 lb |
ASTM D1525 |
Arkema Group LOTADER® 3210 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 3210 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. Main applicationsLOTADER 3210 is a versatile adhesive for extrusi.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | 49 N; ISO 306 |
A.D. Compound Adene NCQAG Copolymer 40% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Vicat Softening Point | 76.0 °C | 169 °F | 50°C/hr; 50N |
Arkema Group Kynar® FLEX 2822 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EDN, N. ?E5.C.H.B.C,, ? (4-8)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousness .. |
|||
Vicat Softening Point | 76.0 - 109 °C | 169 - 228 °F | Average value: 99.0 °C Grade Count:28 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | 50N (T° increase = 5°C/h); ISO 306B50 |
Total Lacqrene® 4801
(discontinued **) LACQRENE® 4801 is an easy flowing, high impact polystyrene for injection molding. The very good processing characteristics of this grade allows for the production of thin articles with long flow p.. |
|||
Vicat Softening Point | 76.0 - 78.0 °C @Load 5.00 kg |
169 - 172 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RKT 736 Rigid PVC, Extrusion Lead Free Transparent antishock profiles |
|||
Vicat Softening Point | 76.0 °C | 169 °F | ASTM D1525 |
C.O.I.M. LARIPUR® LPR7015 Plasticized Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Vicat Softening Point | 76.0 °C | 169 °F | ISO 306B |
Lucite International Elvakon® 4451 Super Low Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable prot.. |
|||
Vicat Softening Point | 76.1 °C | 169 °F | ASTM D1525 |
Teknor Apex Sinvicomp SBF 3758 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact AcceptableUses: Shrink Wrap Forms: Pellets Processing Method: Blown FilmInformation Provided by Teknor Apex |