Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 148 °C | 298 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® BFL2015HF PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only. UL94 V0 1.5 mm for BLACK; V1 1.5 mm for OTHER Color. |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Europe-Africa-Middle East) 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® FXD951A PC Visual effetcs diffusion, flame retardant PC with low/medium flow good for extrusion/injection molding applications. Ideal for light management platforms that require hiding power and transmission.T.. |
|||
Vicat Softening Point | 148 °C @Load 5.10 kg |
298 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1200-15 Polycarbonate Resin Description: LUPOY PC 1200-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Vicat Softening Point | 148 °C @Load 5.10 kg |
298 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1201-15 Polycarbonate Resin Description: LUPOY PC 1201-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Vicat Softening Point | 148 °C @Load 5.10 kg |
298 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1201-18 Polycarbonate Resin Description: LUPOY PC 1201-18 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Vicat Softening Point | 148 °C @Load 5.10 kg |
298 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1300-15 Polycarbonate Resin Description: LUPOY PC 1300-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Vicat Softening Point | 148 °C @Load 5.10 kg |
298 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® F 23 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC 30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/hr, 50N; ISO 306 |
Teijin Panlite® L-1225Y Standard (mold release/ice color grade) Polycarbonate Resin Injection molding and small-sized injection-blow molding grade that require slightly high fluidity. It has an improved mold release property and is bluish-tinted to exhibit clear color.Applications:.. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/hr, 50N; ISO 306 |
Teijin Panlite® LN-1250G Flame Resistant, Translucent Polycarbonate Resin Flame retardant and mold release grade with normal fluidity, which is suitable for injection molding applications.Applications:Electric, electronic and business machine components that need flame re.. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/hr, 50N; ISO 306 |
Teijin Panlite® LN-2250Y Flame Resistant, Translucent Polycarbonate Resin Flame retardant and mold release grade with normal fluidity, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications.Applications:Electric,.. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/hr, 50N; ISO 306 |
Teijin Panlite® LV-2225Y Standard (mold release/ice color grade) Polycarbonate Resin Flame retardant and mold release grade, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications, required to be slightly high fluidity.Appl.. |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Asia Pacific) Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Asia Pacific) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Vicat Softening Point | 148 °C @Load 5.10 kg |
298 °F @Load 11.2 lb |
Rate A (50°C/h); ASTM D1525 |
Styron CALIBREâ„¢ 303V-6 Polycarbonate Resin Overview: CALIBREâ„¢ 303V-6 Polycarbonate resins offer exceptional impact resistance and heat distortion resistance, and meets UL94 V-2 rating. CALIBRE 303V-6 contains a mold release agent, a UV .. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/hr, 50N; ASTM D1525 |
Styron EMERGEâ„¢ 4310-15 Polycarbonate EMERGEâ„¢ PC 4310-15 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq.. |
|||
Vicat Softening Point | 148 °C | 298 °F | B/120; ISO R306 |
Samsung Cheil Industries Infino® SI-3109GL PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 148 °C | 298 °F | ISO 306 |
Polyram RamTough PZ726 Polycarbonate, Impact Modified, UV Stabilized An impact modified, UV stabilized polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Vicat Softening Point | 148 °C | 298 °F | 10N-50°C per hour; ISO 306 |
Total PPH 10099 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 1099 is a controlled-rheology homopolymer having a very narrow molecular weight distribution. PPH 10099 is characterized by high fluidity for high speed spinning on spunla.. |
|||
Vicat Softening Point | 148 °C | 298 °F | ASTM D1525 |
Total PPC 4524WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4524WZ is a nucleated high impact copolymer with a Melt Flow index of 7 g/10 min.TOTAL Polypropylene 4524WZ is characterized by significantly improved impact resis.. |
|||
Vicat Softening Point | 148 °C | 298 °F | ASTM D1525 |
Total PPC 4824WZ Polypropylene, Impact Copolymer ATOFINA 4824WZ is a nucleated impact copolymer. 4824WZ is characterized by improved stiffness and impact resistance, as well as low shrinkage and low warpage. It has been formulated for excellent .. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/h 50N; ISO 306 |
Covestro Makrolon® 1804 Polycarbonate MVR (300 °C/1.2 kg) 6.0 cm3/10 minhigh viscosityUV stabilizedoptimized for low plate-outimproved flammabilityUL 94 V-2/1.5 mm and 3.0 mmavailable in transparenttranslucent and opaque colorssolid sh.. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/h 50N; ISO 306 |
Covestro Makrolon® 3103 MAS157 Polycarbonate ISO 7391-PC,EL,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minExtrusionHigh viscosityUV stabilizedAvailable in color code 550115 onlySolid sheetCorrugated sheetPreprocessingMax. Water conte.. |
|||
Vicat Softening Point | 148 °C | 298 °F | |
Covestro Makrolon® 3103 Polycarbonate Injection molding and extrusion grade with high viscosity, UV stabilized, special grade for sheets.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Baye.. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/h 50N; ISO 306 |
Covestro Makrolon® LTG3123 Polycarbonate PreprocessingMax. Water content |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® 953A PC (Europe-Africa-Middle East) LEXAN 953A is a high viscosity flame retardant, UV-stabilized grade, especially suitable for electrical applications. |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Asia Pacific region. |