Polymer Property : Vicat Softening Point = 172 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 172 °C
342 °F
Rate B; ASTM D1525
Covestro Apec® DP9-9340R High-Heat Polycarbonate, Medical with Release  (discontinued **)
It is the responsibility of the medical device, biological product, or pharmaceutical manufacturer (Manufacturer) to determine the suitability of all component parts and raw materials, including the..
Vicat Softening Point 172 °C
342 °F
Rate B; ASTM D1525
Covestro Apec® DP9-9341 High-Heat Polycarbonate, General Purpose  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Vicat Softening Point 172 °C
342 °F
Rate B; ASTM D1525
Covestro Apec® DP9-9343 High-Heat Polycarbonate, UV Stabilized  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Vicat Softening Point 172 °C

@Load 1.00 kg,
Thickness 4.00 mm
342 °F

@Load 2.20 lb,
Thickness 0.157 in
ISO 306
Solvay Specialty Polymers Solef® 8808/0902 Carbon Fiber Reinforced PVDF Compound  (discontinued **)
Key features of this grade: Carbon Fiber Reinforcement, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinate..
Vicat Softening Point 172 °C
342 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Valox® IQ325 PBT (Asia Pacific)
PBT resin, using chemically recycled post consumer PET Bottles.
Vicat Softening Point 172 °C
342 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Valox® IQ325HP PBT (Asia Pacific)
FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications.
Vicat Softening Point 172 °C
342 °F
ASTM D1525
Toyobo PELPRENE™ S1002 Polyester TPE, Ultra Heat-resistant
Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo.
Vicat Softening Point 172 °C

@Load 5.10 kg
342 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Apec® 1797 High-Heat Polycarbonate
This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along..
Vicat Softening Point 172 °C
342 °F
ASTM D1525
Toyobo Pelprene™ S-1001 Polyester TPE
Key Feature: Pelprene S typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'S' type is a block..
Vicat Softening Point 172 °C
342 °F
Rate B/120; ISO 306
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Europe-Africa-Middle East)
Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom..
Vicat Softening Point 172 °C
342 °F
Rate B/120; ISO 306
SABIC Innovative Plastics NORYL FE8000S PPE+PS
Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom..
Vicat Softening Point 172 °C
342 °F
Rate B/120; ISO 306
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Asia Pacific)
Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom..