Polymer Property : Vicat Softening Point = 204 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 204 °C
399 °F
VST/A/50; ISO 306
GEHR Plastics PA 6 Nylon 6, Dry
Polyamide shows both a high thermostability and high stiffness, hardness and toughness. These are some of the main characteristics. Due to the fact, that the good mechanical characteristics will be ..
Vicat Softening Point 204 °C
399 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics Ultem ATX203R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Vicat Softening Point 204 °C
399 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Ultem ATX203R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Vicat Softening Point 204 °C
399 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Vicat Softening Point 204 °C
399 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Vicat Softening Point 204 °C
399 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Vicat Softening Point 204 °C
399 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Vicat Softening Point 204 °C
399 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East)
VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors.
Vicat Softening Point 204 °C
399 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® 8032U PBT+PET (Europe-Africa-Middle East)
VALOX 8032U is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. Applications: appliance housings, door handles, mirror brackets.
Vicat Softening Point 204 °C
399 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® 8032UX PBT+PET
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
Vicat Softening Point 204 °C
399 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Asia Pacific)
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
Vicat Softening Point 204 °C
399 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® K4560 PBT (Europe-Africa-Middle East)
30% glass reinforced PBT. Impact modified, high flow, hydrolytically stable.
Vicat Softening Point 204 °C
399 °F
B/120; ISO 306
Sax Polymers SAXAMID 126K6 Nylon 6, 30% Glass Filled
SAXAMID 126K6 is a 30% glass beads filled polyamide 6 injection-molding-grade. It is characterized by dimensional stability, low warpage and good surface quality.Information provided by SAX Polymers..
Vicat Softening Point 204 °C
399 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics Noryl GTX GTX965 PPE+PA66
NORYL GTX965 is a mineral reinforced PPE/PA blend. It offers excellent surface appearance, processability and dimensional stability at elevated temperatures. The best molding condition for good appe..
Vicat Softening Point 204 °C
399 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Valox® SHF4340 PBT
20% GF Super High Flow PBT
Vicat Softening Point 204 °C
399 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® SHF4340 PBT
20% GF Super High Flow PBT
Vicat Softening Point 204 °C

@Load 1.00 kg,
Thickness 3.17 mm
399 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
Diamond Polymers DIAMALOY 800 Polycarbonate/Polyester Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Vicat Softening Point 204 °C
399 °F
10 N - A method; ISO 306
Arkema Group Orgalloy® LE 60 ES Polyamide Alloy
Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group
Vicat Softening Point 204 °C
399 °F
10 N - A method; ISO 306
Arkema Group Orgalloy® LE 6000 Polyamide 6 Alloy
Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
Vicat Softening Point 204 °C
399 °F
10 N - A method; ISO 306
Arkema Group Orgalloy® LE60 THM Polyamide Alloy
Polyamide Alloy, Semi-Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
Vicat Softening Point 204 °C
399 °F
(50 °C/h / 50N) - B/50; ISO 306
BASF Ultramid® B50L 01 PA6 (Dry)
Ultramid B50L 01 is a high-viscosity, lubricated, general-purpose extrusion PA6 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendat..
Vicat Softening Point 204 °C
399 °F
(50 °C/h / 50N) - B/50; ISO 306
BASF Ultramid® B27 E 01 PA6 (Dry)
Ultramid B27 E 01 is a low viscosity general-purpose, extrusion PA6 grade well suited for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German..
Vicat Softening Point 204 °C
399 °F
ASTM D1525
Samyang Triel® 5700 Thermoplastics Polyetherester Elastomer, General Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5700 is an extrusion grade.Information provided by Samyang.