Polymer Property : Vicat Softening Point = 224 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 224 °C
435 °F
Rate A/50; ASTM D1525
SABIC Innovative Plastics Valox® V8030CS PBT+PET
Glass filled Valox with enhanced surface
Vicat Softening Point 224 °C
435 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics NORYL GTX GTX8408 PPE+PA
Noryl GTX* GTX8408 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is glass filled and suitable for injection molding. The elongation of this material is higher than GTX8410W..
Vicat Softening Point 224 °C
435 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL GTX GTX8408 PPE+PA
Noryl GTX* GTX8408 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is glass filled and suitable for injection molding. The elongation of this material is higher than GTX8410W..
Vicat Softening Point 224 °C
435 °F
Rate B/120; ISO 306
SABIC Innovative Plastics NORYL GTX GTX8408 PPE+PA
Noryl GTX* GTX8408 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is glass filled and suitable for injection molding. The elongation of this material is higher than GTX8410W..