Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 224 °C | 435 °F | Rate A/50; ASTM D1525 |
SABIC Innovative Plastics Valox® V8030CS PBT+PET Glass filled Valox with enhanced surface |
|||
Vicat Softening Point | 224 °C | 435 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL GTX GTX8408 PPE+PA Noryl GTX* GTX8408 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is glass filled and suitable for injection molding. The elongation of this material is higher than GTX8410W.. |
|||
Vicat Softening Point | 224 °C | 435 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX8408 PPE+PA Noryl GTX* GTX8408 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is glass filled and suitable for injection molding. The elongation of this material is higher than GTX8410W.. |
|||
Vicat Softening Point | 224 °C | 435 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX8408 PPE+PA Noryl GTX* GTX8408 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is glass filled and suitable for injection molding. The elongation of this material is higher than GTX8410W.. |