Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 127 °C @Load 1.00 kg |
261 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Eraclene® FA 706 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 706 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Films manufactured with Eraclene FA 706 show good processability t.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS (Europe-Africa-Middle East) Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS High impact PC+ABS material designed for local Pacific Automotive applications |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525B |
SABIC PP681K Polypropylene Random Copolymer for Injection Molding Product Description: PP 681K is specially developed for producing injection molded articles with high clarity and also has better impact properties than homo PP counterparts.PP 681K has the followi.. |
|||
Vicat Softening Point | 127 °C @Load 5.001 kg |
261 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH GF4030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
Chevron Phillips HiD® 9354 HDPE Natural Pipe Resin
(discontinued **) Resin Type: gas phase linear hexane copolymerApplications: corrugated pipe applicationsInformation provided by Chevron Phillips Chemical Company. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
Chevron Phillips HiD® 9720 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear homopolymerCharacteristics: good flow, moderate impact strength, excellent stiffness, moderate ESCR, moderate shrinkage resistanceApplications: pails, structural foamInformation p.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
LyondellBasell Alathon® L5332CP High Density Polyethylene, Blow Molding Grade ALATHON L5332CP is bimodal molecular weight distribution, fractional melt index HDPE resin that exhibits an exceptional balance of environmental stress crack resistance and stiffness. Typical applic.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
LyondellBasell Alathon® L5440 High Density Polyethylene ApplicationsALATHON L 5440 is designed for high shear machines. It exhibits excellent color, low odor and excellent processing stability. Typical applications include general purpose, household ch.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
LyondellBasell Alathon® M5370PX High Density Polyethylene, Extrusion Grade ALATHON M5370PX is a copolymer with a narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processability. T.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
LyondellBasell Petrothene® LR734001 High Density Polyethylene (Sheet & Profile Extrusion) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
LyondellBasell Petrothene® LR734045 High Density Polyethylene (Sheet & Profile Extrusion) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Europe-Africa-Middle East) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER F-1 weathering certified in natural color, specially designed for Pool & Spa applications. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER (Asia Pacific) F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS (Asia Pacific) NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Asia Pacific) Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ISO 306 |
Borealis FS1560 High Density Polyethylene FS1560 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Films made of FS1560 have high impact and tensile strength, and bala.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ISO 306 |
Total 5502 HDPE, blow molding, pipe Drug Master File listed; USP Class VI approved; FDA compliant; UL 94HB/746 certified |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
ExxonMobil HDPE AS55-03 High Density Polyethylene Resin Product Description: AS55-003 is a blow molding grade high density polyethylene copolymer containing an antistatic additive. It provides a good balance of stiffness and stress crack resistance.Avail.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
ExxonMobil HDPE BU46-055 High Density Polyethylene Resin Product Description: BU46-055 is a high molecular weight, high density polyethylene copolymer which contains a UV inhibitor. It possesses a combination of excellent processability, outstanding melt .. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
NOVA Chemicals Sclair® D916-39 HDPE Extrusion Resin
(discontinued **) Features: Excellent processability, excellent stretchability, high stiffness, superior strength, gel free, excellent UV resistance.Applications: Industrial woven bags, tarpaulins.Data provided by th.. |
|||
Vicat Softening Point | 127 °C @Load 1.00 kg |
261 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Eraclene® MM 84 U High Density Polyethylene - Injection Molding Eraclene MM 84 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 84 U is characterized by high rigidity and good impac.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xylex HX7409HP PC+POLYESTER (Asia Pacific) Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI).. |
|||
Vicat Softening Point | 127 °C @Load 1.02 kg |
261 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem RP 145 RACO Random Polypropylene Copolymer RP 145 is a high melt flow rate random copolymer designed for use in thin-walled injection molding parts. This product offers good transparency, very good stiffness/impact strength balance, excellen.. |