Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 157 °C | 315 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 153 PC (Asia Pacific) Nonhalogenated. 2.5 MFR. Blowmolding/extrusion. UV-stabilized. |
|||
Vicat Softening Point | 157 °C | 315 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 153R PC Nonhalogenated. 2.5 MFR. Blowmolding/extrusion. UV-stabilized. Internal mold release. |
|||
Vicat Softening Point | 157 °C | 315 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® 4251R PPC+PC High heat polycarbonate copolymer blend with an excellent balance of heat resistance, processability, and impact strength. Available in a range of opaque colors. |
|||
Vicat Softening Point | 157 °C | 315 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® 4401R PPC+PC (Europe-Africa-Middle East) LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 157 °C | 315 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® 4404 PPC+PC High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi.. |
|||
Vicat Softening Point | 157 °C | 315 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® 4404 PPC+PC (Asia Pacific) High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi.. |
|||
Vicat Softening Point | 157 °C | 315 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® 4404 PPC+PC (Europe-Africa-Middle East) High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi.. |
|||
Vicat Softening Point | 157 °C | 315 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® FXD153 PC FXD153 is an Extrusion / Blow molding grade in a Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Co.. |
|||
Vicat Softening Point | 157 °C | 315 °F | ASTM D1525 |
PolyMirae Moplen HP640N Injection Molding Grade Polypropylene Moplen HP640N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP640N is a homopolymer particularly suitable for injection molding.. |
|||
Vicat Softening Point | 157 °C | 315 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® RL7517 PC FDA compliant (color limited). 2.5 MFR. Potable water/extrusion blowmolding applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 157 °C | 315 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® 151 PC (Asia Pacific) Nonhalogenated. 2.5 MFR. Blowmolding/extrusion.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 157 °C | 315 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® FXD941A PC FXD153 is an Extrusion / Blow molding grade in a Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Co.. |
|||
Vicat Softening Point | 157 - 205 °C | 315 - 401 °F | Average value: 178 °C Grade Count:27 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
Vicat Softening Point | 157 °C | 315 °F | A120; ISO 306 |
Inno-Comp INNOPOL® CS 1-6140 N 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-6140 N is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-6140 N is developed for producing injection molded components for household eq.. |
|||
Vicat Softening Point | 157 °C | 315 °F | ASTM D1525-97 |
Ipiranga Petrochem PH 0141 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Vicat Softening Point | 157 °C | 315 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ4860HR PBT Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Vicat Softening Point | 157 °C | 315 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Asia Pacific) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Vicat Softening Point | 157 °C | 315 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Asia Pacific) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Vicat Softening Point | 157 °C | 315 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Asia Pacific) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Vicat Softening Point | 157 °C | 315 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Europe-Africa-Middle East) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Vicat Softening Point | 157 °C | 315 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Europe-Africa-Middle East) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Vicat Softening Point | 157 °C | 315 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Europe-Africa-Middle East) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Vicat Softening Point | 157 °C | 315 °F | |
Styron CALIBRE™ 200 6 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Vicat Softening Point | 157 °C | 315 °F | |
Styron CALIBRE™ 300 6 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Vicat Softening Point | 157 °C | 315 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Noryl PKN4717 PPE+PS (Asia Pacific) PPE+PS. Translucent. FDA compliant. High heat. Foam extrusion. Microwavable. Food packaging uses. Solid properties listed.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 157 °C | 315 °F | A50 (10N); ISO 306 |
Domo 1040RC Polypropylene Homopolymer Information provided by Domo. |
|||
Vicat Softening Point | 157 °C | 315 °F | 50 N; ISO 306 |
Azoty Tarnow™ TARNOFORM 300 K POM Tribological modified grade with addition of special chalk, which causes decrease of wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Vicat Softening Point | 157 °C | 315 °F | B |
Plastcom SLOVALEN PH 82 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Vicat Softening Point | 157 °C | 315 °F | 10N, 50°C/hr; ISO 306 |
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1030 PP SABIC® PPcompound 19T1030 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding applications... |