Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 235 °C | 455 °F | B |
Plastcom SLOVAMID 6/66 GF 50 PA6/66, 50% glass fibre FeaturesPA 6/66 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-g.. |
|||
Vicat Softening Point | 235 °C | 455 °F | 9.8 N; ISO 306, ASTM D1525 |
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr.. |
|||
Vicat Softening Point | 235 °C | 455 °F | 49 N; ASTM D1525 |
Nilit Polynil® C50L Externally Lubricated PA66/6 Description: Polynil C50L shows better surface finish, flow and elongation than a comparable homopolymer. Key characteristics: Excellent flowHigh elongationGood impact strengthGood overall mechanica.. |
|||
Vicat Softening Point | 235 °C @Load 5.10 kg |
455 °F @Load 11.2 lb |
50°C/h |
Radici Radilon® A RCF3505 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Vicat Softening Point | 235 °C | 455 °F | ISO 306 |
Radici Radilon® AERV1906 LK (dry) Nylon 66 Glass-fiber reinforced with high impact strength, heat stabilizedInformation provided by Radici group. |
|||
Vicat Softening Point | 235 °C @Load 5.00 kg |
455 °F @Load 11.0 lb |
|
LATI Latamid 66 H2E21 G/13 PA 66, 13% Glass Fiber Reinforced Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. Glass fibers. High impact resistance. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific;.. |
|||
Vicat Softening Point | 235 °C @Load 5.00 kg |
455 °F @Load 11.0 lb |
|
LATI Latamid 66 H2 G/25-V0KB PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Vicat Softening Point | 235 °C | 455 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® V9260CS PET (Asia Pacific) Color Stable Glass filled PET |
|||
Vicat Softening Point | 235 °C | 455 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® V9260CS PET (Europe-Africa-Middle East) Color Stable Glass filled PET |
|||
Vicat Softening Point | 235 °C | 455 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® V9260DCS PET (Europe-Africa-Middle East) Color Stable Glass Filled PET (for Dark colors only) |
|||
Vicat Softening Point | 235 °C | 455 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® V9280LW PET (Europe-Africa-Middle East) 40% Glassfiber / Mineral Filled PET, Impact Modifier, Mold Release, Heat StabilizedThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 235 °C | 455 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® V9290 PET (Europe-Africa-Middle East) 45% GF PET, Glass, Mold Release, Heat Stabilized, |
|||
Vicat Softening Point | 235 °C | 455 °F | B/120; ISO 306 |
Sax Polymers SAXAMID 226K6 Nylon 6.6, 30% Glass Beads SAXAMID 226K6 is a polyamide 6.6 injection-molding-grade filled with 30% glass beads. It is characterized by optimized shrinkage properties.Information provided by SAX Polymers |
|||
Vicat Softening Point | 235 °C | 455 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX8120P PPE+PA (Europe-Africa-Middle East) GTX8120P is a glass filled extrudable Noryl GTX with low thermal conductivity, suitable for thermal breaks |
|||
Vicat Softening Point | 235 °C | 455 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX8120P PPE+PA (Europe-Africa-Middle East) GTX8120P is a glass filled extrudable Noryl GTX with low thermal conductivity, suitable for thermal breaks |
|||
Vicat Softening Point | 235 °C | 455 °F | B/120; ISO 306 |
Sax Polymers SAXAMID 236F4Q32 Nylon 6.6, 20% Glass Fiber SAXAMID 236 F4Q32 is a impact-modified polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers and very good flow properties. It is suitable for applications requiring toughness in co.. |
|||
Vicat Softening Point | 235 °C | 455 °F | B/120; ISO 306 |
Eurostar Starflam AFR682A1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR682A1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 235 °C | 455 °F | B/50; ISO 306 |
Eurostar Starflam AFR682A1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR682A1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 235 °C | 455 °F | B/120; ISO 306 |
Eurostar Starflam AFR682B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR682B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 235 °C @Load 5.10 kg |
455 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NA40 GR14 NL MC PA6.6, 14% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 235 °C @Load 5.10 kg |
455 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NA40 GR30 NL IH PA6.6, 30% glass fiber reinforced, impact modified, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 235 °C @Load 5.10 kg |
455 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NA40 GR13 NL100 MB PA6.6, 13% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 235 °C @Load 5.10 kg |
455 °F @Load 11.2 lb |
50°C/h |
Radici Radilon® A 35E 990 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Vicat Softening Point | 235 °C | 455 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® V9230CS PET (Europe-Africa-Middle East) 15% GF PET Injection Moulding grade, Heat and Color Stabilised, for light colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 235 °C | 455 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East) Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |
|||
Vicat Softening Point | 235 °C | 455 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East) Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |
|||
Vicat Softening Point | 235 °C | 455 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East) Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |
|||
Vicat Softening Point | 235 °C @Load 5.00 kg |
455 °F @Load 11.0 lb |
|
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion .. |
|||
Vicat Softening Point | 235 °C @Load 5.00 kg |
455 °F @Load 11.0 lb |
|
LATI Latamid 66 H2 G/25-V0KB4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |