Polymer Property : Vicat Softening Point = 554 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 290 °C
554 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105-7568/GY PEEK, with PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Superheated steam sterilizable.High chemical resistance parts, hydrolysis resistance, non ..
Vicat Softening Point 290 °C
554 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 19-7276 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Vicat Softening Point 290 °C
554 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 19-7319 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Vicat Softening Point 290 °C
554 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 19-7416 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Vicat Softening Point 290 °C
554 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 19-7669 Polyamide 46, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot..
Vicat Softening Point 290 °C
554 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 46/CF/15 Polyamide 46, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® 46HF4130 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® 46HF5041LW Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® TE200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® TE250F3 Nylon 46-15% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® TE341 Nylon 46 (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® TW200F3 Nylon 46-15% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® TW200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® TW200F8 Nylon 46-40% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® TW200FM33 Nylon 46-30% Glass and Mineral Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® TW241F10 Nylon 46-50% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® TW241F12 Nylon 46-60% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® TW271F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® TW300 Nylon 46 (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® TW371 Nylon 46 (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® TW441 Nylon 46 (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie..
Vicat Softening Point 290 °C

@Load 5.10 kg
554 °F

@Load 11.2 lb
ISO 306
Eurotec® Tecomid® NT40 GR30 NL HS PPA, 30% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® TW341 Nylon 46 (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Vicat Softening Point 290 °C
554 °F
Average value: 290 °C Grade Count:16
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® TE250F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Vicat Softening Point 290 °C
554 °F
50°C/h 50N; ISO 306
DSM Stanyl® 46HF5050 Nylon 46-50% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..