Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Recommended |
Nye Lubricants NC-140 Grease Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
Precision Polymer Engineering V72H Fluoroelastomer Compound Fluoroelastomer Rubber, 65-75 °IRHD. FDA grade. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Food and Drug Admi.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Z50B Hydrogenated NBR Compound Hydrogenated Nitrile Rubber, 45-55 °IRHD. Medium acrylonitrile (ACN) content. ASTM designation = HNBR. To meet ASTM D2000 line call-out 2MDH508, A26, B16, EO16, EO36, F14, Z1, where Z1 = tensile s.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Z75G Hydrogenated NBR Compound Green Hydrogenated Nitrile Rubber, 70-80 °IRHD. Medium acrylonitrile (ACN) content. ASTM designation = HNBR. ASTM D2000 line call-out 2MDH708, A26, B36, EO16, EO36, F14, Z1. Z1 = hardness 75 ±5... |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Z75Y Hydrogenated NBR Compound Yellow Hydrogenated Nitrile Rubber, 70-80 °IRHD. Medium acrylonitrile (ACN) content. ASTM designation = HNBR. ASTM D2000 line call-out 2MDH708, A26, B36, EO16, EO36, F14, Z1. Z1 = hardness 75 ±5.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Z90B Hydrogenated NBR Compound Peroxide cured, Hydrogenated Nitrile Rubber, 85-95 °IRHD. Medium acrylonitrile content (ACN = 36%). ASTM designation = HNBR. To meet ASTM D2000 line call-out M2DH920, A26, B16, EO16, EO36, F14.Ap.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Gehman T100 |
Zeon Chemicals HyTemp® 4051CG AR Polyacrylate Elastomer HyTemp 4051CG contains acrylic esters with a small percentage of a chlorine/carboxy cure site monomer. Vulcanizates have excellent oil, heat and compression set resistance.Cement grade version of Hy.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Gehman T100 |
Zeon Chemicals HyTemp® 4051EP AR Polyacrylate Elastomer HyTemp 4051EP contains acrylic esters with a small percentage of a chlorine/carboxy cure site monomer. Vulcanizates have excellent oil, heat and compression set resistance.Easy processing version of.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
ConocoPhillips Tacna® HD Grease NLGI Grade 1 Tacna HD is a premium quality, adhesive, extreme-pressure (EP) lithium complex grease developed for the lubrication of heavily loaded construction, mining and industrial equipment. It also is recomm.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | See Note 1. |
ChevronTexaco Crater® Fluid H Texaco Crater lubricants delivers value through:Low environmental impact — Contains a carrier solvent that is a non-ozone depleting diluent.Good water resistance — Strong resistance to water washo.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | See Note 1. |
ChevronTexaco Molytex® EP NLGI Grade 0 Texaco Molytex EP grease delivers value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading, extending vehicle .. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | See Note 1. |
ChevronTexaco Molytex® EP NLGI Grade 2 Texaco Molytex EP grease delivers value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading, extending vehicle .. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
ChevronTexaco RPM® NLGI 1 Automotive LC Grease EP FeaturesChevron RPM Automotive LC Grease EP is a water resistant, extreme pressure, heavy duty chassis, wheel bearing and general purpose lubricating grease. It is manufactured using highly refined,.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
ChevronTexaco RPM® NLGI 2 Automotive LC Grease EP FeaturesChevron RPM Automotive LC Grease EP is a water resistant, extreme pressure, heavy duty chassis, wheel bearing and general purpose lubricating grease. It is manufactured using highly refined,.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | TR test, TR10 |
Daikin DAI-EL G-704 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | TR test, TR10 |
Daikin DAI-EL G-723 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Excellent mold releasability, non-sticking.Information provided by Dai.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | TR test, TR10 |
Daikin DAI-EL G-763 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Excellent mold releasability for O-rings.Information provided by Daiki.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | TR test, TR10 |
Daikin DAI-EL G-783 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Fast vulcanization, for complex shapes.Information provided by Daikin .. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | See Note 1. |
ChevronTexaco Starplex® Premium NLGI Grade 1 Texaco Starplex Premium delivers value through:Continuous high temperature stability up to 325°F.Excellent corrosion and wear protection.Excellent water resistance.Extended relubrication intervals .. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
3M 4516 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Application |
3M FM019602 MC Polyester Label Products 3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Application |
3M FM0196J MC Polyester Label Products 3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
3M 3302 Specialty Foil Tape Aluminum foil tape. EMI/RFI shielding. Ul 510 Recognized.Information provided by 3M |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
3M 4116 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Application |
3M FM0196J MC Polyester Label Product 3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Application |
3M FM05540K MC Polyester Label Product 3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Application |
3M FV022902 Soft White Vinyl Label Product 3M™ Soft White Vinyl Label Product FV22902 is a flexible vinyl label stock that offers excellent durability and some moisture resistance. This vinyl label utilizes 3M™ Adhesive F2201 which is a fr.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
3M 4718 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
3M Scotch® Super 33+™ Vinyl Electrical Tape Scotch® Super 33+™ Vinyl Electrical Tape is a premium grade, 7 mil thick, all-weather vinyl-insulating tape. It is designed to perform continuously in ambient temperatures up to 105°C. The tape i.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | See Note 1. |
ChevronTexaco Crater® CSF Texaco Crater lubricants delivers value through:Low environmental impact — Contains a carrier solvent that is a non-ozone depleting diluent.Good water resistance — Strong resistance to water washo.. |