Polymer Property : Minimum Service Temperature, Air = 29.7 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -1.30 °C
29.7 °F
Gehman torsion test, T2
Daikin DAI-EL G-603 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 71% Fluorine Content
Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Information provided by Daikin Industries.
Minimum Service Temperature, Air -1.30 °C
29.7 °F
Gehman torsion test, T2
Daikin DAI-EL G-901 Fluoroelastomer Terpolymer, Peroxide Curable Grade, 71% Fluorine Content
Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Excellent solvent resistance.Information provided by Daikin Industries.
Minimum Service Temperature, Air -1.30 °C
29.7 °F
Gehman torsion test, T2
Daikin DAI-EL G-902 Fluoroelastomer Terpolymer, Peroxide Curable Grade, 71% Fluorine Content
Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Excellent solvent resistance, good mold flow.Information provided by Daikin Industries.