Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS NOVODUR® L3FR ABS, Injection Grade
(discontinued **) Injection molding grade, flame retardant, very easy flow. Contains no polyhalogenated diphenyls or diphenyl ethers.Applications: Television and computer housings.Information provided by the manufact.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Oroglas® DRT Acrylic, Impact Grade
(discontinued **) For extrusion and injection molding applications. OROGLAS DRT combines good thermal resistance with an excellent impact resistance.Key features : impact resistance: up to 10 times more impact-resis.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Halar® 300DA Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Halar® "DA" grades are available and meet the FDA's Condition of Use B, as described under 21 C.F.R. 176-170(c).Information provided by Solvay Specialty Polymers. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Halar® 350LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Halar® 500LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 23.0 - 55.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Lanxess Durethan® BC 30 S 000000 Nylon 6 PA 6, non-reinforced, injection moldingInformation provided by LANXESS. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® CI 31 F 000000 Copolyamide PA6/6I Copolyamide PA6/6I, low melt point (188-191°C), low viscosity, no additives, very high transparency, in compliance with FDA as far as the PA-layer is separated from the food by a 50 µm PE film.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® KU 2-7604 000000 PBT+PC PBT+PC, non-reinforced, injection molding, extrusion, flame retardant, impact modified, low tendency to warp |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | |
Solvay Specialty Polymers Halar® 300DA Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Halar® "DA" grades are available and meet the FDA's Condition of Use B, as described under 21 C.F.R. 176-170(c).Features: Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 .. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | |
Solvay Specialty Polymers Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation prov.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | |
Solvay Specialty Polymers Halar® 930LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
Styrolution NOVODUR® P2MC ABS, Injection Grade Injection molding grade for plating; very good ratio between toughness, heat resistance and flow.Applications: All parts to plating: e.g. sanitary parts. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 23.0 - 80.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
Styrolution Terblend® N NM-19 XP Beige 38163 ABS+PA (Dry) Description: Terblend® N NM-19 XP is an UV stabilized ABS/PA blend combining very high impact strength, even at low temperatures with an outstanding processability and excellent surface appearanc.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® XE 4128 black 9221 PA610 Product description: Grilamid XE 4128 black 9221 is a modified high viscosity Polyamide 610 for extrusion as well as injection molding. A characteristic of tubes made out of this material is the hig.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact ApplicationsZytel FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been develop.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature -40.0 - 23.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 100PE NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE NC010 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions... |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature -40.0 - 23.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 103FHSA NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHSA NC010 is a heat stabilized lubricated polyamide 66 for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® AECN TL Nylon 12, Cable Sheathing Grade (Conditioned) Designation ISO 1874-PA12,KHL,14-010Extrusion grade for the sheathing of wires and cables. Available colors: natural and orange. Heat and light stabilized.Low melt viscosity. High speed extrusion. V.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® AMV TL Nylon 12, Rigid, Injection Grade (Conditioned) Designation ISO 1874-PA12,MHLR,16-010Rigid grade for injection molding. Available color: natural. Light and heat stabilized. Mold-release agent.High impact strength. Easy filling of the mold due to .. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
BASF Polystyrol® 432 B Impact Grade Polystyrene (Europe) Very easy-flowing, low impact grade for parts with unfavorable flow path/wall-thickness ratios.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
BASF Polystyrol® 455 F WU Impact Grade Polystyrene (Europe) Very easy-flowing, impact-modified grade.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
BASF Procom® X5S 770 Polypropylene Car bumpers and spoilers where good paintability is required.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® BESN P20 TL Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11-P,EHL,22-004Flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.Flexibility. High impact strength. Very good chemical resistan.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
BASF Polystyrol® 454 C Impact Grade Polystyrene (Europe) Easy flowing, medium-impact grade.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K223-P2 Impact Modified Nylon 6 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |