Polymer Property : CTE, linear, Parallel to Flow = 30.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 - 30.0 µm/m-°C

@Temperature 50.0 - 100 °C
11.1 - 16.7 µin/in-°F

@Temperature 122 - 212 °F
ISO 11359-2
Raschig Group AMPLA® 2000 melamine-modified polyester
Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve..
CTE, linear, Parallel to Flow 20.0 - 30.0 µm/m-°C

@Temperature 50.0 - 100 °C
11.1 - 16.7 µin/in-°F

@Temperature 122 - 212 °F
ISO 11359-2
Raschig Group AMPLA® 2500 melamine-modified polyester
Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Excellent elasticity and shock resistance, low post-shrinkage, very good electrical values, high heat..
CTE, linear, Parallel to Flow 20.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit 3640 CG Novolac Phenolic
Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par..
CTE, linear, Parallel to Flow 20.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 68.0 °F
Vyncolit G885 Novolac Phenolic
Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Information provided by Vyncolit, a Sumitomo Bak Group
CTE, linear, Parallel to Flow 20.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit X681 Novolac Phenolic
Glass fiber filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction. Tribological compound with PTFE additive.USES: Water pump seals and self-lubrica..
CTE, linear, Parallel to Flow 20.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit 2950 W Novolac Phenolic
Mineral and glass fiber filled phenolic molding compound with a very high strain to failure in flexure. UL listed.USES: Armature insulation.Information provided by Vyncolit, a Sumitomo Bak Group
CTE, linear, Parallel to Flow 20.0 - 30.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT
Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation..
CTE, linear, Parallel to Flow 20.0 - 30.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Dry)
Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability.
CTE, linear, Parallel to Flow 20.0 - 30.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Dry)
Description: 30% glass-fiber reinforced injection-molding grade with enhanced hydrolysis resistance, e.g., for applications in vehicle cooling systems.Information provided by BASF
CTE, linear, Parallel to Flow 20.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit X682 Novolac Phenolic
Glass fiber, glass bead and graphite filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction.USES: Water pump seals and self-lubricating bearings.Info..
CTE, linear, Parallel to Flow 20.0 - 30.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultradur® B 4040 G10 50% Glass Filled BK 15029 PBT + PET
Description: Injection molding grade with 50% glass fibers for industrial parts with excellent surface quality, for example external door handles in vehicles, visible sunroof frames, oven door handl..
CTE, linear, Parallel to Flow 20.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit 3520 CG Novolac Phenolic
Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par..
CTE, linear, Parallel to Flow 20.0 - 30.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultradur® B 4300 G6 LT 30% Glass Filled BK 150926 PBT
Description: Easy flowing injection molding grade with 30 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg windshield wiper arms, printed circuit boards PCBs), housing, ..