Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
17.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP JFL34 PES
LNP* LUBRICOMP* JFL34 is a compound based on Polyethersulfone resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant.
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature 23.0 - 85.0 °C
17.8 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Solvay TECHNYL® C 216 V30 PA6, 30% glass fiber, DRY
Description: Polyamide PA6, reinforced with 30 % of glass fiber, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: It has good mechanical properties, it is used..
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature 23.0 - 85.0 °C
17.8 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, DRY
Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers..
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature -30.0 - 100 °C
17.8 µin/in-°F

@Temperature -22.0 - 212 °F
ISO 11359-2
SABIC Innovative Plastics SABIC PPCOMPOUND 8620A PP
SABIC® PPcompound 8620A is a mineral filled, impact modified polypropylene TPO. It was originally designed for painted automotive bumper fascia applications where a combination of good flow, hig..
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature 23.0 - 85.0 °C
17.8 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Solvay TECHNYLSTARâ„¢ S 216 V30 PA6, 30% glass filled, DRY
Description: TECHNYL STAR TM Polyamide, reinforced with 30% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific, Europe and North AmericaPr..
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
17.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Lubricomp RFN16SXS PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RFN16SXS is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Euro..
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
17.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP SCP36 PA12
LNP* LUBRICOMP* SCP36 is a compound based on Nylon 12 containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant, Electrically Conductive.
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
17.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp CF004 PS (Europe-Africa-Middle East)
LNP* Thermocomp* CF004 is a compound based on Polystyrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DF006HL PC
LNP THERMOCOMP* DF006HL is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Low Extractible, Healthcare.
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
17.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP RF006SXZ PA 66
LNP* THERMOCOMP* RF006SXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this material is: Heat Stabilized.
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
17.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP RF008 PA 66
LNP* THERMOCOMP* RF-1008 is a compound based on Nylon 66 resin containing Glass Fiber.
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
17.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP WF006 PBT (Europe-Africa-Middle East)
LNP* THERMOCOMP* WF006 is a compound based on Polybutylene Terephalate resin containing Glass Fiber.
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
17.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP ZFM3314 PPE (Europe-Africa-Middle East)
glas, mineral filled PPE
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
17.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOTUF MF0049I PP (Europe-Africa-Middle East)
LNP* THERMOTUF* MF0049I is a compound based on Polypropylene resin containing Glass Fiber, Flame Retardant. Added features include; Flame Retardant, Chemically Coupled.
CTE, linear, Parallel to Flow 32.0 µm/m-°C
17.8 µin/in-°F
ASTM E831
Sumitomo Bakelite North America E 9405H-1 Glass Filled Electrical Encapsulation Grade Epoxy
E-9504H-1 is glass fiber filled epoxy molding compound designed for encapsulation of delicate electrical components as well as large coils. Excellent thermal shock, moldability, and retention of ele..
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
17.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP NF0061 PC+ABS (Europe-Africa-Middle East)
LNP* THERMOCOMP* NF0061 is a compound based on PC+ABS resin containing Glass Fiber, Flame Retardant. Added features include : Flame Retardant.
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
17.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP RF008XXH PA 66
LNP* THERMOCOMP* RF008XXH is a compound based on Nylon 66 resin containing 40% Glass Fiber. Added feature of this material includes: Healthcare.
CTE, linear, Parallel to Flow 32.0 µm/m-°C
17.8 µin/in-°F
dry; ISO 11359-1/-2
DSM EcoPaXX® Q-KG6 PA410-GF30
% Glass Reinforced, Heat Stabilized, for E&E applications
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature 20.0 - 93.3 °C
17.8 µin/in-°F

@Temperature 68.0 - 200 °F
Parallel to Laminate
CIP Composites 200 Series Laminated Polymer Bearing Material
The 200 series consists of PTFE/polyester combination fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated ma..
CTE, linear, Parallel to Flow 32.0 µm/m-°C
17.8 µin/in-°F
dry; ISO 11359-1/-2
DSM EcoPaXX® Q-HG6 PA410-GF30
30% Glass Reinforced, Heat Stabilized
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature 20.0 - 93.3 °C
17.8 µin/in-°F

@Temperature 68.0 - 200 °F
Parallel to Laminate
CIP Composites 100 Series Laminated Polymer Bearing Material
The 100 series consists of polyester fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated material. Laminated..
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
17.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starflam BFR330A PA6, Glass Bead Reinforced, Flame Retardant, Injection Molded
Starflam BFR330A is a Flame Retardant, Glass Bead Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Parallel to Flow 32.0 µm/m-°C
17.8 µin/in-°F
ISO 11359
BASF Petra® 110 BK-112 15% Glass Filled PET
Petra 110 is a 15% glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a good combination of performance properties including good strength a..
CTE, linear, Parallel to Flow 32.0 µm/m-°C
17.8 µin/in-°F
ISO 11359
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Dry)
Ultramid 8234G HS is a heat stabilized, 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensio..
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature 20.0 °C
17.8 µin/in-°F

@Temperature 68.0 °F
ISO data
BASF Capron® 8234G 44% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8234G is a 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is ..
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
17.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP KF006 POM (Europe-Africa-Middle East)
LNP* THERMOCOMP* KF006 is a compound based on Acetal Copolymer resin containing Glass Fiber
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
17.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON KX97157 Acetal Copolymer (Europe-Africa-Middle East)
LNP* STATKON* KX97157 is a compound based on Acetal resin containing Carbon. Added features include : Electrically Conductive, Impact Modified.